Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.

I agree, do not show this message again.

Solubility of oxygen in (TeO2)0.78(WO3)0.22 glass melt

S. V. SMETANIN1, G. E. SNOPATIN1, M. F. CHURBANOV1,*

Affiliation

  1. Institute of Chemistry of High-Purity Substances of the Russian Academy of Sciences, 49 Tropinin St., GSP-75, Nizhny Novgorod 603950, Russia

Abstract

The solubility of oxygen in (TeO2)0.78(WO3)0.22 glass melt at 640оС by the use of technique based on the measurement of oxygen pressure over the melt in evacuated closed system has been studied. The solubility of oxygen at pressure of 3.9×103 Pa over the melt is equal to (5.6 ± 0.6)×10-6 mole/cm3 . A linear increase of solubility is observed in the pressure range from 1000 to 5000 Pa and the effective Henry coefficient is 5×108 Pa/mole/cm3..

Keywords

Tellurite glass melt, Solubility of oxygen, TeO2 – Wo3, Henry’s law.

Submitted at: Dec. 2, 2008
Accepted at: Jan. 29, 2009

Citation

S. V. SMETANIN, G. E. SNOPATIN, M. F. CHURBANOV, Solubility of oxygen in (TeO2)0.78(WO3)0.22 glass melt, Journal of Optoelectronics and Advanced Materials Vol. 11, Iss. 1, pp. 41-44 (2009)